Precious metals - recovery & refining - a DIY approach Know


36:26
Cupellation - from cupel to SILVER bead
04:40
The BEST SMB GOLD drop so far
24:44
GOLD and SILVER extraction from ceramic CPUs and silver contacts - recovery & refining
12:59
3kg SILVER bar
11:25
melting pure 24K (99.99%) GOLD buttons
19:11
24K (99.99%) pure GOLD: the refining process PART 2
21:58
24K pure GOLD 99.99%: the refining process PART 1
13:58
GOLD from Intel Pentium Pro: yields, recovery and refining PART 3
20:07
GOLD alloyed with PALLADIUM and SILVER: parting and refining
07:42
SILVER melting and casting
09:03
GOLD from Intel Pentium Pro: yields, recovery and refining PART 2
05:23
GOLD from Intel Pentium Pro: yields, recovery and refining PART 1
13:45
GOLD yield: the last 6 CPUs from the 5kg batch
08:14
GOLD yield from 10 IBM 686 and 10 Cyrix 686 ceramic CPUs
17:20
How much gold in 10 AMD 386 ceramic CPUs?
14:54
GOLD yield from 10 AMD K5 ceramic CPUs
10:14
GOLD recovery from 2kg mixed ceramic CPUs
10:36
SILVER contacts de-soldering new method
24:32
GOLD recovery from fountain pen nibs with iodine
12:28
1kg AMD 486 ceramic CPUs GOLD yield
02:40
Ceramic CPUs: 5kg mix for GOLD recovery
07:44
GOLD from 5kg intel 386 & 486 ceramic CPUs PART 7: total yield
22:55
GOLD from 5kg intel 386 & 486 ceramic CPUs PART 6: processing the lids
12:00
GOLD from 5kg intel 386 & 486 ceramic CPUs PART 5: GOLD from residues
18:33
GOLD from 5kg intel 386 & 486 ceramic CPUs PART 4: washing and melting
08:57
GOLD from 5kg intel 386 & 486 ceramic CPUs PART 3: dissolution & precipitation
14:48
SILVER stripping cell - sodium sulphite electrolyte PART 2
07:57
GOLD from 5kg intel 386 & 486 ceramic CPUs PART 2: crushing
07:14
GOLD from 5kg Intel 386 & 486 ceramic CPUs PART 1: preparation
14:58
SILVER stripping cell - sodium sulphite electrolyte PART 1
14:35
GOLD extraction from transistors with iodine PART 2 of 2
19:20
GOLD extraction from transistors with iodine PART 1 of 2
01:38
Using a bench shear to prepare transistors for GOLD extraction with iodine
11:49
GOLD recovery from 10 ceramic AMD Duron CPUs
40:40
Refining GOLD to 24K (99.99%) - inquarting & reduction with oxalic acid - full process
20:51
VERY high yield GOLD plated pins
23:01
GOLD recovered from 8.9 kg gold fingers: the results
09:20
GOLD fingers test run: 6g Au from 1 kg fingers
17:59
PALLADIUM reduction with formic acid
22:59
From dirty solution to fine SILVER bar
07:06
CuCl2 etched GOLD plated pins: the results
10:14
Remelting SILVER from formic acid refining
13:00
melting pure SILVER , refined with formic acid
25:34
From dirty AgNO3 to 9999+ pure SILVER with formic acid
16:08
PALLADIUM melting (no time lapse)
32:21
PALLADIUM and SILVER parting
22:25
Refining GOLD to 99.99% (24K) with oxalic acid
12:07
Experiment: processing MLCCs for PALLADIUM, SILVER and GOLD recovery PART 1
12:16
Refining GOLD foils from pins after recovery with AP
08:25
DIY: gas-fired foundry
17:18
refining GOLD slime full process
19:46
stripping GOLD plated pins electrolysis test
10:56
SILVER contacts recovery - running large batches
08:12
Iodine - GOLD extraction from ceramic CPU
12:34
Transistors GOLD leaching with iodine
21:35
GOLD plated contacts full process PART 2
23:53
GOLD plated contacts full process PART 1
12:39
SILVER from silver chloride - lye and sugar method
06:49
SILVER bar marking - quick and easy
08:05
GOLD plated pins in thiourea - citric acid electrolyte